论文部分内容阅读
对以Fe73 5Cu1Nb3 Si13 5B9为代表的非晶合金的原带和经 5 2 0℃等温退火处理的样品以及激波处理样品作了对比DSC分析。着重结合晶化机理对样品在上述处理中的晶化速率作了对比和讨论。
The DSC analysis of the original band of amorphous alloy represented by Fe73 5Cu1Nb3 Si13 5B9 and the sample annealed at 520 ℃ and the shock-treated samples were compared. Focus on the crystallization mechanism of the sample in the above-mentioned crystallization rate were compared and discussed.