论文部分内容阅读
研究了Fe77.5-x-yCuxNbySi13.5B9合金(x=0.1;y=0~3)经低温长时间等温退火后合金元素(Cu和Nb)对品化的影响。发现非晶带在低于300℃退火时形成a-Fe(Si)纳米品,晶粒尺寸取决于合金化学成分和热处理条件.发现,Fe77.5Si13.5B9合金即使在300℃退火晶粒也生长,400℃时?
The effect of alloying elements (Cu and Nb) on the quality of Fe77.5-x-yCuxNbySi13.5B9 alloy (x = 0.1; y = 0 ~ 3) after low temperature isothermal annealing was studied. A-Fe (Si) nanomaterials were found to form when the amorphous zone annealed below 300 ° C. The grain size is dependent on the chemical composition of the alloy and the heat treatment conditions. Found that, Fe77.5Si13.5B9 alloy even at 300 ℃ annealing grain growth, 400 ℃?