论文部分内容阅读
Ti-Al 复合板的生产包括在钛坯上放置(搭接)已加热到300~500℃的铝坯,并且对其进行压力焊接(收缩率 r%为637.5T~(-0.555)或(?)1822T~(-0.798),T 为铝坯的加热温度)。在压力焊接过程中,钛坯的反
The production of Ti-Al composite plates consists of placing (overlapping) an aluminum billet that has been heated to 300-500 ° C on a titanium blank and subjecting it to pressure welding (shrinkage r% 637.5T -0.555) ) 1822T ~ (-0.798), T is the heating temperature of aluminum billet). In the pressure welding process, titanium billet counter