论文部分内容阅读
Al-8.5Fe-1.3V-1.7Si alloy was prepared by spray deposition and hot extrusion. The high temperature plastic deformation behavior of the spray deposited Al-8.5Fe-1.3V-1.7Si alloy was investigated in the strain rate range of 2.77×10-4-2.77×10-2 s-1