论文部分内容阅读
绪言目前一般对含贵金属较高的硫化铜矿,通过火法处理,使贵金属经冰铜后富集于铜阳极泥中,再进行回收。但是,火法流程不可避免地会产生SO_2气体及有害微尘,使环境受到污染,且对含铅、锌高的复杂铜矿难于处理。而氯盐浸出湿法炼铜不仅对这类铜矿的适应性较大,又能控制对环境的污染,但对其中贵金属的回收是否理想,都是人们十分关注的问题。本文着重讨论CuCl_2氯盐溶液浸出湿法炼铜过程中回收贵金属的问题。 INTRODUCTION At present, copper sulfide ores containing higher noble metals are generally treated by fire to make the precious metals be enriched in copper anode slimes after matte addition and recovery. However, the pyrometallurgical process inevitably generates SO 2 gas and harmful fine dust, pollutes the environment, and is difficult to handle for complex copper mines containing lead and zinc. Chloride leaching wet-process copper is not only more adaptable to such copper ore, but also can control the pollution of the environment, but whether the recovery of precious metals is ideal or not is a problem of great concern to people. This article focuses on the CuCl_2 chloride solution leaching wet-process copper recovery precious metals.
其他文献
从1916年开始的湿法炼锌,实际上还包括硫化精矿的焙烧和浸出渣的烟化等火法冶金过程。1968年采用热酸浸出以后,浸出渣的烟化在许多工厂已被湿法浸出所替代。1981年,加 Zinc
一、锡矿的类型和成分我厂处理的复杂錫矿包括:高錫鎢矿精选产出的副产品錫尾矿和原矿略經粗选的毛錫矿。錫的品位較低,均含有鎢、鉍、銅、鉛、钼、铁、砷、硫和硅等杂质。
用2-乙基-1-己基磷酸单2-乙基-1-己基脂(M2EHPA)从硫酸镍溶液中分离钴的方法进行了研究。M2EHPA的分离系数比D2EHPA大很多倍(D2EHPA是熟知的一种阳离子交换萃取剂)。 使用3级
大屯矿每年约产出1.5万吨铜锌精矿,送冶炼厂与一般铜精矿配料熔炼。结果是伴生有价金属锌、铟、镉、铋回收率很低,甚至无法回收,而且给造锍熔炼本身带来了困难。 因此,寻求
锡矿中经常有铁存在,氧化铁与锡石共生,二者以细粒晶体相互嵌布。当前选矿方法很难将二者较完全地分开,锡精矿中就难免有铁,有时含铁量不少。锡与铁共存于锡精矿中,还原熔烁
目前我国铜电解精炼中所采用的添加剂——明胶(动物胶)和水胶(植物胶)——是有很大缺点的。首先这两种胶的电极极化是异常大的,而且电极极化是随其浓度增大而增大的,所以槽
铝酸钠溶液碳酸化分解是燒结法生产氧化铝的重要工序之一。碳酸化分解的条件对氧化铝的质量和分散度有重大影响。二氧化硅在铝酸钠溶液碳酸化分解过程中的行为,对分解有着巨
我厂净化处理铜电解液的方法,采用结晶硫酸铜——电积脱铜的流程。长期以来,仅从电积脱铜母液中沉淀析出无水硫酸镍和回收硫酸。在深入开展“工业学大庆”的群众运动中,我厂