The mechanical properties of magnesium alloys at both ambient and elevated temperatures can be improved with the existence of Mg2Si phase in the matrix.However,these properties can be deteriorated if the Mg2Si phase is of coarse Chinese script type.Effects of the silicocalcium addition on the microstructure and properties of an Mg-6Al-0.5Mn alloy(AM60)were studied.The microstructure of the alloy with the addition of silicocalcium is featured with dispersedly distributed small polygonal type Mg2Si phases.The microhardness,tensile strength,percentage elongation and toughness of as-cast AM60+1.0Si-Ca alloy are 20%,13.3%,28.5% and 50% higher than these of AM60 alloy respectively.Further corrosion measurements showed that the silicocalcium-modified AM60 alloy increases the corrosion potential by 0.04V and decreases the lost weight corrosion rate by 45%. The mechanical properties of magnesium alloys at both ambient and elevated temperatures can be improved with the existence of Mg2Si phase in the matrix. However, these properties can be deteriorated if the Mg2Si phase is of coarse Chinese script type. Effects of the silicocalcium addition on the microstructure and properties of an Mg-6Al-0.5Mn alloy (AM60) were studied. The microstructure of the alloy with the addition of silicocalcium is featured with dispersedly distributed small polygonal type Mg2Si phases. microhardness, tensile strength, percentage elongation and toughness of as-cast AM60 + 1.0Si-Ca alloys are 20%, 13.3%, 28.5% and 50% higher than these of AM60 alloys respectively. Future corrosion measurements showed that the silicocalcium-modified AM60 alloy increases the corrosion potential by 0.04V the lost weight corrosion rate by 45%.
其他文献
M42(W2Mo9Cr4VCo8)钢是一种近年由国外引进的钼系超硬性高速钢,用于加工难切削的材料。国内生产的和国外引进的这种钢材在材料质量上有一定的差异,而对它的热处理参数又掌握
八十年代末中国居民经济福利的分配李实[瑞典]古斯塔夫森一、导言现实中的中国正在发生着从集中的计划经济体制向市场经济体制这样一种巨大的制度变革。这种变革过程不仅意味着
一、前言 球形接头是直升飞机上发动机架的重要零件。它共有五种形式,其中一种如图1所示。其他四种,有的水平接头在零件相应位置的另一端,方向相反;有的如图1A-A剖面上的斜
前言对生物医学用金属材料耐体液腐蚀的要求很高。在一般工程技术应用中,把腐蚀速度为25.4微米/年的材料称为耐蚀性极好的材料。但在医学上,要求金属材料的腐蚀速度等于或少
测定合金中相的阳极极化曲线,过去常用粉末压型法、导电胶法,它们或因粉末用量太多,或因手续繁琐等而有一定的局限性。为此我们设计制造了“粉末电极”,用它测定了大量提取相
国家地震局根据当前地震形势,提出地震预报方法实用性研究的课题,并采用攻关的形式,目标明确,注重实效,注重应用。我们认为,这是继各种预报方法清理之后的又一重要战役,将对
高如曾(1984)在“预测油气富集的数理统计法”一文中认为,模糊领域的信息统计量似乎更适应描述地震信息量的特征。但是,该法计算过程繁杂,不便应用。本文依据高如曾提供的38
iSuppli公司对今年经济增长的预期要比2006年低得多。虽然经济增长放慢,但由于消费市场、通讯市场和汽车市场的需求旺盛,从而支持了全球经济保持强劲。电子元器件终端产品不
一、前言蠕虫状石墨铸铁具有一些独特的机械及物理的综合性能,并已广泛地被用来制造钢锭模、气缸盖、排气管、剎车鼓及液压阀零件。同时对这一材料的显微组织特点以及石墨形