狂犬病又叫恐水症,是由狂犬病毒引起的急性传染病,属于人畜共患性传染病,可对人体中枢神经系统产生损害,一旦发病,病死率高达100%[1]。狂犬病暴露指被狂犬、疑似狂犬和或不确定是否健康的其他狂犬宿主动物抓伤、咬伤、舔舐破损皮肤处或黏膜,也指黏膜、开放性伤口受到可能感染了狂犬病病毒的动物组织或唾液[2-3]。温州经济发达,商贸活动频繁。为了解温州市区人群狂犬病暴露伤害状况,制定狂犬病防治 Rabies, also known as fear of water disease, is an acute infectious disease caused by rabies virus, belonging to zoonotic infectious diseases, may cause damage to the central nervous system, once the onset, the case fatality rate as high as 100% [1]. Rabies exposure refers to scratching, biting, licking or damaging the skin or mucous membranes of rabies, suspected rabies and other rabid host animals that are not yet known for their health. The open wounds are also affected by rabies virus-infected animal tissues or Saliva [2-3]. Wenzhou economy developed, frequent commercial activities. In order to understand the population risk of rabies in Wenzhou city, make rabies prevention and control
其他文献
  本文提出了采用水化影响因子Eh以表征辅助胶凝材料对水泥水化的作用,并建立了其计算模型。文章采用水化影响因子研究了掺合料对水泥水化的促进或抑制作用。
  在固定的加热制度下,本文系统地研究了掺加不同种类、不同含量掺合料的水泥基材料在700℃高温后的力学性能,得出了每种掺合料在水泥基材料中的最优掺量以及对水泥基材料
  本文试验研究了经活化处理并磨细的煤矸石以不同比例等量替代部分水泥后,对掺减水剂水泥浆体流动度的影响规律,并将煤矸石与常用的活性矿物掺合料矿渣粉、高钙粉煤灰进行
  碳化是一般大气环境下混凝土中钢筋脱钝锈蚀的前提条件,从而影响混凝土结构的耐久性。本文研究了掺高活性稻壳灰和硅灰混凝土的碳化过程,测定了混凝土的碳化深度和氢氧化
迄今为止,我国个人住房抵押贷款的不良率在1%左右,是商业银行不良贷款率最低的信贷业务。按照国际经验,个人住房抵押贷款的风险暴露期为3至8年。随着我国个人住房抵押贷款业
  本文采用再生粗集料以不同比例取代天然集料的同时,用矿渣、粉煤灰等活性掺合料等量取代水泥,研究了掺活性掺合料再生混凝土的力学性能和耐久性能。实验结果表明,随再生
机器状态的有效监控是保障机器安全运行、提高制造系统生产效率的重要途径 .由于环境的复杂性与不确定性 ,现有机器故障诊断系统的可靠性还不能满足应用要求 ,为此近年来发展
  本文采用压汞法研究了在超塑化剂存在条件下,钢渣、矿渣、粉煤灰三种磨细矿物掺合料单掺及复掺对水泥石孔结构特征的影响.研究结果表明,水化早期三种矿物掺合料单掺或复
  研究了钢渣微粉对混凝土路用性能和抗冻融循环能力的影响,结果表明:掺钢渣微粉可使混凝土路用性能和抗冻性能大幅度提高,当钢渣微粉掺量10%时,其抗折强度比普通基准混凝土提高
  本文研究了徐州未燃煤矸石以石膏和萤石作矿化剂煅烧前后结构性能变化及其活化机理。研究结果表明:掺加的氧化钙被大量消耗;不同配比和热历史对煤矸石活性影响程度不同,但