Y7520W螺纹磨砂轮修整器的改进

来源 :机械工人.冷加工 | 被引量 : 0次 | 上传用户:wilsonpfan
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
Y7520W万能螺纹磨床砂轮修整器,为手动式修整器。使用这种修整器,要求操作者在修整砂轮时非常仔细,如果手动速度过快和不均匀,都会在砂轮型面上留下锯齿形的沟痕,从而影响了被加工零件的表面粗糙度。经分析产生锯齿形沟痕的主要原因是:由于磨床砂轮直径较大,转速较低,就决定了修整器手动速度不能太快。而机床原砂轮修整器手动机构为1:1杠杆传动,所以很难达到均匀和慢速。为此,我们对原修整器做了以下改进。 Y7520W universal thread grinder wheel dresser, manual dresser. The use of such dressers requires the operator to be careful when dressing the grinding wheel. If the manual speed is too fast and uneven, it will leave a zigzag groove on the grinding wheel surface, affecting the surface roughness of the part being machined. Analysis of the sawtooth-shaped groove marks the main reason is: due to the grinding wheel diameter larger, lower speed, it determines the dresser manual speed can not be too fast. The original machine wheel dresser manual mechanism for the 1: 1 lever drive, it is difficult to achieve uniform and slow. To this end, we made the following improvements to the original trimmer.
其他文献
第四讲锻件对锻模寿命的影响在工业生产中,尽管锻件的品种和规格变化无穷,但是,无论锻造什么样的锻件,锻模总是存在着相应的损坏规律。了解这种规律,将有助于锻模的选材、设
一、前言对于把金相学作为控制热处理质量的工具这一见解,我们主要从它用来对工业上广泛使用的大型开模锻钢件进行热处理控制的观点进行讨论。热处理的质量控制,在某些方面,
本文对30CrMnSi在焊接时易产生冷、热裂纹,从理论上进行了分析,并介(?)为防止裂纹,在焊接薄壁容器时,所采取的工艺措施及试验规范参数。 In this paper, 30CrMnSi easy to p
本刊工作会议于8月16日至20日在新疆生产建设兵团召开,来自全国二十三个省、市、自治区及部分中央国家机关和国有大中型企业的政研会会长、秘书长、党委书记、宣传部长及优
她,是一个极其普通的农妇。与千千万万的农民一样,一辈子追求着生活。然而,旧社会的反动制度摧残了她,不得不以乞讨谋生。社会主义制度建立后,她曾得到过极大的幸福生活,也
本文通过扫描电子显微镜来研究轴承钢接触疲劳试验过程中和实际推力轴承使用过程中疲劳剥落行为。一、试验用料和试验方法试验料为轴承钢GCr15和实际推力轴承外圈。疲劳寿命
经典形核理论告诉我们,当新相自母相中形核时,总自由能变化为其中-△G_▼为单位体积自由能的变化,V为新相的核心体积,A为表面自由能(其与曲率无关),A为新相生成所增加的表面
7CrSiMnMoV钢是84年由首钢与第二汽车厂共同研制成功的新型冷作模具钢。该钢淬透性好,热处理变形小,在硬度相同的条件下抗弯、抗压及冲击韧性高于CrWMn及Cr12MoV钢,但耐磨性
(接上期)十三、擒腕别肘的用法待敌式:见图1。敌我双方呈虚步,敌左手左腿在前,右手持刀。我方右臂微屈约呈90度,两手自然握拳,前脚掌着地,含胸收腹,气沉丹田。(图41)敌出左直
本文对9Cr18、GCr15及Cr12MoV三种钢材在离子注氮、气体氮化、离子氮化以及淬火等不同工艺处理后,轻负荷下的抗磨损性能进行了研究。发现离子注氮后的试样抗磨损性能最佳,并