侧面粘贴钢板加固混凝土梁试验,是一项用来测试钢板加固后的梁的抗剪性能的试验。由试验可知,侧面粘贴钢板加固后的钢筋混凝土梁能有效提高抗剪强度,同时也提高了抗弯强度和刚度。而且抗剪强度随着钢板厚度和宽度的增加而随之增长。在试验中,粘贴钢板的梁比未粘贴钢板梁的抗剪强度提高很多,最高达到了84%。文章探讨了侧粘钢板加固钢筋混凝土破坏机理,为研究钢筋混凝土侧粘钢板加固设计理论打下基础。 Side-bonded steel plate reinforced concrete beam test, is used to test a steel plate reinforced shear performance test. It can be seen from the test that the reinforced concrete beam reinforced by the side-glued steel plate can effectively improve the shear strength and simultaneously increase the flexural strength and rigidity. And the shear strength increases with the increase of the thickness and width of the steel plate. In the tests, the shear strength of the bonded steel beams was much higher than that of the unbonded steel beams up to 84%. The paper discusses the failure mechanism of reinforced concrete with side-sticking steel plate, which lays a good foundation for the research on reinforcement design theory of reinforced concrete side sticking steel plate.
其他文献
随着人们对环境质量要求的不断提高和2008年奥运会的临近,绿化、美化、净化首都环境的任务变得十分艰巨。目前,外来有害生物入侵、危险性林木病虫扩散、生态平衡失调等问题给
在常压及不同O_2-N_2气相组成下,曾对Cu在氨性溶液中的溶解动力学进行了研究. 溶解系电化学反应过程,溶解速度为阴极过程控制时,控制因数是氧的传递;为阳极过程控制时,控制因
参加会议的有来自北京市、地矿部、城乡建设部、中国科学院、兵器工业部、高等院校等廿一个单位的有关专家33人。会上,围绕北京城市特点、性质、市情、建设需要,城市发展战
知识产权主要分为二大部份:工业产权(包括专利,商标,商业秘密等)和版权(著作权,经济学家称其为易逝产权)。知识产权制度保证了以上两部分内容得以实施。本文主要讨论的是高校
随着工业的发展,对无缝钢管的需要日趋迫切。德国的曼乃斯曼兄弟于1884年提出了用周期轧制法制造无缝钢管的设想。1892年在德国建成了第一台周期式轧管机。实践证明,周期轧
Al-Mg-Si合金的双级时效特性比Al-Zn-Mg合金更复杂,所以适用于Al-Zn-Mg合金的洛里默尔——尼科尔森(Lorimer-Nicholson)模型就不适用于Al-Mg-Si合金。然而,目前所提出的各种
40岁以上人群为原发性高血压多发人群,是临床上常见的心脑血管疾病。随着社会的快速发展,人们生活水平也得到了很大改善,但由于人口老龄化、饮食结构变化和食盐摄入量的增加,
经过林业专家的调查研究,首都绿化委员会办公室最近向社会公布了刚刚确定的北京市主要造林树种。侧柏、国槐、雪松等100多种树木被列为京城绿化的“主力军”,它们将在北京今
本文初步探讨了氢诱发裂纹作为一种环境诱发缺陷在材料破坏过程中的作用。结果表明,作为一级近似,氢诱发裂纹可视为一组平行于轧制面的面缺陷,它对材料的常规强度指标影响不
近半个世纪,铝在钢中有两个大不相同的脱氧常数,已由世界范围内的研究者用资料所反复证实。例如,在1600℃,Kd=(%Al)~2(%O)~3值经测定为10~(-14)或10~(-9),这取决于试验如何做