Fast Degradation of Green Pollutants Through Nanonets and Nanofibers of the Al-Doped Zinc Oxide

来源 :金属学报(英文版) | 被引量 : 0次 | 上传用户:hanyikuaile1112
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
In this study,series of nanolayered structures of Zn-Al LDHs were prepared by urea hydrolysis.Nanofibers and nanonets of the Al-doped ZnO were formed via the decomposition of the nanolayers under high pressure and temperature.Nanospheres were also prepared for comparison.The different morphologies of the prepared nanomaterials were confirmed by several techniques.An improvement for the optical properties of the doped zinc oxides was observed through narrowing of their band gap energies because of transforming the nanolayers to nanonets and nanofibers.The photocatalytic activities of the prepared nanomaterials were studied through photocatalytic degradation of the pollutants of acid green dyes.Complete decolorization and mineralization of green dyes happened in the presence of the nanolayers and nanospheres within 4-6 h,while the nanonets and the nanofibers achieved the complete decolorization and degradation of the dyes at shorter time 1.3 h.These results could be explained though the kinetic study of the photocatalytic degradation of dyes.It was concluded that the nanonets and the nanofibers were very effective for the photocatalytic degradation of pollutants.
其他文献
Immiscible alloys have aroused considerable interests in the last decades on account of their special physical and mechanical properties and potential applications.A considerable number of researches have been implemented to investigate the solidification
Hot deformation behavior of a high Al-low Si transformation-induced plasticity (TRIP) steel was studied by an MMS-300 thermo-simulation machine at the temperature range of 1050-1200 ℃ and strain rate range of 0.01-10 s-1.The constitutive equations of the
In a fusion reactor,plasma-facing components (PFCs) will suffer severe thermal shock;behavior and performance of PFCs under high heat flux (HHF) loads are of major importance for the long-term stable operation of the reactor.This work investigates the the
The composition and structural evolution of the corrosion product film of two commercial 90Cu-10Ni tubes,namely Tube A and Tube B,after being immersed in natural seawater for 1,3,and 6 months were characterized by scanning electron microscopy,energy-dispe
The effect of thermal aging on phase transformation and impact toughness of an as-cast duplex stainless steel was investigated at room temperature.After long-term thermal aging,the impact toughness decreases significantly and the cracks initiate and propa
The fracture of pipelines caused by corrosion cracks and the resulting oil and gas leakage can lead to great environmental pollution and economic losses.These negative effects are due to serious corrosion of the plain carbon steels used for armor of flexi
The strain rate sensitivity (SRS) and temperature sensitivity (TS) of 316L austenitic stainless steel were investigated by constant strain rate test (CSRT) and strain rate jump test (SRJT) under four temperatures (293,373,473 and 573 K) and four strain ra
Three-dimensional parts of the 30CrMnSiA steel were successfully fabricated using selective laser melting (SLM).The microstructures and mechanical properties of the SLM-processed 30CrMnSiA samples were investigated by scanning electron microscope and tran
The crevice corrosion behaviors of 436 stainless steels in chloride-containing solutions with sulfate addition were studied using potentiodynamic,galvanostatic and repassivation potential measurements.The results of these electrochemical tests were compar
The hot deformation behavior and processing map of Cu-bearing 2205 duplex stainless steel (2205-Cu DSS) were investigated at temperatures of 950-1150 ℃ and strain rates of 0.01-10 s-1.The effects of Cu addition and different deformation parameters on defo