论文部分内容阅读
这种起动的方法是把鎂电解槽装滿廢电解质进行起动。其特点是为了改善劳动卫生条件和縮短电解槽起动时間,往电解槽中加的廢电解质中氯化鎂含量小于3.5%,当电解质溫度达到680℃以后,再逐漸提高氯化鎂的含量。
The starting method is to fill the magnesium electrolyzer waste electrolyte to start. Its characteristic is to improve the sanitation conditions and shorten the start-up time of the electrolyzer. The content of magnesium chloride in the waste electrolytes added to the electrolyzer is less than 3.5%. When the electrolyte temperature reaches 680 ° C, the content of magnesium chloride is gradually increased.