本文是钽—10%钨合金高温短时抗氧化涂层探索实验报告。提出了在1800~1900℃下对合金具有几分钟保护能力的三种涂层体系及实验情况。
This article is tantalum-10% tungsten alloy high temperature short-term anti-oxidation coating to explore the experimental report. Three kinds of coating systems and their experimental conditions were proposed to protect the alloy from several minutes at 1800-1900 ℃.