Isothermal corrosion (γ'+γ) Ni3Al alloy in liquid zinc

来源 :中国有色金属学会会刊(英文版) | 被引量 : 0次 | 上传用户:blue1234sky
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
The isothermal corrosion testing and microscopic examination of Ni3Al alloy in liquid zinc containing small amounts of aluminum (mass fraction less than 0.2%) at 450 ℃ were carried out. The results show that the controlling mechanism of the dissolution reaction is diffusion through a boundary layer into liquid zinc. For two-phase alloy, Ni3Al alloy (γ+γ), the interface between dissolving solid and liquid remains remarkably planar and the difference in dissolution of the two adjacent phases (γ+γ) can not be experimentally observed. The boundaries between γ phase and γ phase play no perceptible role in the dissolution of Ni3Al alloy in liquid zinc. The X-ray diffraction spectra of the diffusion layer confirm the presence of Ni5Zn21. The corrosion rate of the Ni3Al alloy in molten zinc was calculated to be approximately 2.6×10-3 g/(cm2-h), therefore the liquid zinc corrosion resistance of Ni3Al alloy is very weak.
其他文献
Large eddy simulations (LES) of mixing process in a stirred tank of 0.476m diameter with a 3-narrow blade hydrofoil CBY impeller were reported. The turbulent fl
The sound absorption property of aluminum foam was studied by testing its sound absorption coefficients using standing wave tube method. The open-pore aluminum
Bamboo-like carbon nanotubes were synthesized by ethanol catalytic combustion (ECC) technique with combustion method. Copper plate was employed as substrate,eth
Magnesium alloy AZ91 was prepared by powder metallurgy method, and the effect of sintering temperature on the densities and microstructures of the alloys was in