The true stress-strain curves of compressed ZK60 alloy have two typical characters. Most thermal simulation compressing curves of ZK60 have the obvious character that around 0.2 in strain the stress reaches the peak and declines rapidly afterwards and lands the lowest. The decline of the curve illustrates that the test specimen has been destroyed and crackles can be found on the test specimen correspondingly. And the other true stress increases to a peak and then decreases to a steady state, indicating that dynamic recrystallization has occurred in ZK60 alloy. From the analysis of the results we can receive the optimized composite of the deformed parameters and get the reasonable deformed temperatures to be 200 ℃ or 400 ℃, which can play a directing role in determining the deforming technology of wrought magnesium alloys.
其他文献
The microstructure of the as-cast, as-solution-treated and as-aged wrought magnesium alloy ZK60 was studied. The results indicate that the microstructure of the
The effects of heat treatment on the microstructure and compressive properties of porous Ni-rich NiTi shape memory alloy (SMA) fabricated by self-propagating hi
The springback is one of the key factors which affect the forming quality of thin-walled tube NC precision bending. The elastic-plastic finite element method wa
For developing high performance magnesium alloys, a new method in combination of B2O3 addition and melt stirring was applied. When 0, 3%, 6% and 12%( mass fract
The deformation and damage mechanism of aluminum alloy (6063) were investigated by 0°, 30°, 45°, 60° and 90° tensile tests and tensile-unload tests with th
The effect of 5%Cr(mole fraction) on the scaling behavior of Ni-10Al was investigated at 900 ℃ and 1 000 ℃ with the aim to discuss the third element effect(TE
The experiments of continuous and directional solidification of titanium alloys with cold crucible were carried out in a multifunctional electromagnetic cold cr
Rapid solidification method was employed to produce TiAl based alloy ribbons and finally to produce TiAl based alloys with novel microstructure and properties.
Polycrystalline bulk Ti3AlC2 material with high purity and density was fabricated by hot pressing from the powder mixture with the starting stoichiometric mole
As-cast AZ91+XCa (X=0, 0.5%, 1.0%, 1.5%, mass fraction) magnesium alloys were extruded into tube at 380℃ with an extrusion ratio of 6:1. The tensile properties