A diamond single crystal, which was synthesized at a high temperature of 1570 K and a high pressure of 5.5 GPa in a Fe-Ni-C system, was directly and systematica
In order to realize the co-firing with Ag/Pd electrodes in multilayer devices, Pb(Zn1/3Nb2/3)1-,-yZrxTiyO3(0.25<x<0.35, 0.25<y<0.35) piezoelectric ceramics (hereaft