The transformation and dissolution of Mg(Zn, Cu, Al)2 phase during solution treatment of an Al–Zn–Mg–Cu alloy containing high zinc were investigated by means
7055 aluminum alloy plates with the same size were rolled by two processes: small percentage reduction per pass (PRPP) and large percentage reduction per pass,