论文部分内容阅读
目前转炉炼钢成渣速度慢,初渣碱度低,熔炼时间长,炉衬寿命低。为了提高转炉炉龄,公司安排我厂试验室进行合成渣试验研究,为工业试验提供条件和依据。随后公司又决定在我厂一烧1~#、2~#烧结机上进行工业试验,在车间和公司有关处及运输部的大力支持和配合下,于77年8月2日连续进行了11个小时的工业试验,共生产了转炉合成渣29车,计1194吨,获得了圆满的结果。
At present, the converter slag into slag slow, early slag alkalinity is low, melting a long time, low lining life. In order to improve the furnace furnace age, the company arranged for our laboratory test laboratory synthetic slag for industrial testing to provide the conditions and basis. Subsequently, the company decided to carry out industrial tests on the 1 #, 2 ~ # sintering machines in our plant. With the strong support and coordination from the relevant departments of the workshop and the company and the Ministry of Transport, the company conducted 11 consecutive inspections on August 2, Hours of industrial testing, a total of 29 vehicles produced converter slag, weighing 1194 tons, and achieved satisfactory results.