近几年来,我在工程验收及工程回访中发现,墙面抹灰反碱是一个弊病不太大而占比例较多又普遍发生的问题,有些工程在交工使用后不久便出现反碱,使乳胶漆或油漆咬色、变色,起皮脱落,有些工程还拖延了工期。
In recent years, I have found during construction acceptance and engineering visits that plastering and anti-alkali on the wall is a problem that is not too serious, and that it accounts for a large proportion of the problems. It is common that some projects occur shortly after the completion of the work, making anti-alkali so that Latex paint or paint bite, discoloration, peeling off, some projects also delay the duration.