1概况我厂现有9台中压煤粉锅炉,担负着为氧化铝生产供汽的主要任务,其中9#炉为UG-160/3.82-M型锅炉,于2003年开始建设,2004年5月13日准备并汽试运行,但在并汽后逐渐带负荷过程中,汽温急剧由420℃降低到300℃以下,尝试3次均因同样原因并汽失败。经过在并汽过程中对参数的分析,最终确定了并汽失败的原因,进行了处理,于2004年5月31日正常并汽。2锅炉蒸汽系统9#炉为单锅筒自然循环锅炉,过热器由顶棚管、 1 Overview Our existing 9 sets of medium-pressure pulverized coal boilers, responsible for the production of alumina for the main steam supply, of which 9 # furnace UG-160 / 3.82-M-type boiler, started construction in 2003, May 2004 On the 13th, it was prepared and run on a steam test. However, during the gradual load-carrying process after the co-vaporization, the temperature of the steam suddenly dropped from 420 ° C to below 300 ° C. Three attempts were made to fail the same reason. After the process of gas and the parameters of the analysis, and ultimately determine the cause of FAW failure, was processed, in May 31, 2004 and normal steam. 2 boiler steam system 9 # boiler for a single drum natural circulation boiler, superheater by the roof tube,
其他文献
本文介绍了薄管板和小径厚壁换热管结构的双管板换热器制造难点,围绕确保换热管与内管板强度胀接质量而制造了有效的工艺措施,保证了产品质量.
本文介绍了大型循环流化床锅炉整体水压试验的方法和程序。 This paper introduces the method and procedure of the overall hydrostatic test of large-scale circulatin
在能效测试和锅炉运行现状分析的基础上,对一台SZL15-1.25-AII型锅炉热效率偏低进行了分析。针对锅炉运行过程中存在的排烟温度高、炉渣可燃物含量高、受热面结垢及水处理工
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生、测量监控等方面人手,介绍了S226海滨大桥
7月19日,世界第二台、国内第一台30万千瓦的CCPP机组在鞍钢正式竣工投产。这项具有节能、环保、发电多重功能的燃气蒸汽联合循环发电机组工程的建成投产,标志着鞍钢的高炉煤
本测评系统为无纸化的考试测评系统,实现了对于考试流程中从题目上传、检查、审核到题库生成,试卷创建,以及学生答题、考场监控、试卷评阅的整个过程.主要开发语言为C#语言并
密封性能差的托辊,轴承很容易被污染使托辊出现“早期失效”。托辊与胶带之间就会由理想的滚动摩擦转变为非正常的半滚动半滑动摩擦,随着托辊污染程度的增加,滚动逐渐变差,直
油、气站场和大型储备库地下钢制管道及金属构筑物的阴极保护较长输管道要复杂的多,本文结合工程案例并依据投运后的实测实量数据,对多种保护方案进行了对比分析,提出站场阴
本文简述了锆材的物理性能和化学性能,重点介绍了工业纯锆(Zr-3,R60702)在容器制造过程中应注意的事项,如筒体卷制中变形,焊接工艺及复合材料的焊后检验方法,供同行交流参考