利用激光冲击波对X80管线钢焊接接头表面进行了强化处理,通过拉伸实验对激光冲击处理前后焊接接头试样拉伸力学性能进行了分析,用扫描电镜和能谱分析仪观察了其断口形貌与化学成分组成,并对其断裂机理进行了探讨。实验结果表明,原始状态的X80管线钢焊接接头具有连续屈服特征,无明显的屈服平台,延伸率比较高,拉伸断口出现明显的分层开裂;激光冲击处理后X80管线钢焊接接头的强度并未得到加强,韧窝尺寸与深度变大,其断裂拉伸性能得到改善。 The laser shock wave was used to strengthen the surface of welded joint of X80 pipeline steel. The tensile mechanical properties of welded joint before and after laser shock treatment were analyzed by tensile test. The fracture appearance of the welded joint was observed by SEM and EDS And chemical composition, and its fracture mechanism was discussed. The experimental results show that the welded joints of X80 pipeline steel in the original condition have the characteristics of continuous yielding, no obvious yield platform, relatively high elongation and obvious delamination cracking at the tensile fracture; the strength of X80 pipeline steel welded joints after laser shock treatment Unconfirmed, dimple size and depth become larger, and its tensile properties at break are improved.
其他文献
由于抗反转录病毒治疗(antiretroviral therapy,ART)在人类免疫缺陷病毒(human immunodeficiency virus,HIV)感染人群中的有效开展,获得性免疫缺陷综合征(acquired immunodeficien
针对太阳辐照度测量仪器高性能及微型化的要求,研究了一种绝对辐射计的关键器件———微机电系统(MEMS)微型红外辐射探测芯片。该芯片以在红外宽光谱范围内具备高吸收率的镍
针对聚合物电致发光二极管(PLED)面光源的结构特点,建立了PLED面光源正负极双通道的散热模型。采用有限元分析软件对PLED面光源在光强为1000 cd/m2时的热特性进行模拟,获得其