7075铝合金高温流变行为的研究

来源 :热加工工艺 | 被引量 : 0次 | 上传用户:aaron209
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
采用圆柱试样在 Gleeble- 15 0 0热模拟机上进行高温压缩变形实验 ,研究了 70 75铝合金在高温塑性变形过程中流变应力的变化规律。实验在温度为 2 5 0~ 5 0 0℃、应变速率为 0 .0 5~ 5 0 s- 1的条件下进行。结果表明 :应变速率和变形温度的变化强烈影响着合金流变应力的大小 ,流变应力随变形温度升高而降低 ,随应变速率提高而增大 ;可用 Zener-Hollomon参数的双曲正弦形式来描述 70 75铝合金高温压缩变形时的流变应力行为 Cylindrical specimens were subjected to high-temperature compression deformation on a Gleeble-1500 thermal simulator to study the variation of flow stress during the high temperature plastic deformation of 7075 aluminum alloy. The experiment was carried out at a temperature of 250 ~ 500 ℃ and a strain rate of 0.05 ~ 500 s-1. The results show that the change of strain rate and deformation temperature strongly influence the flow stress of the alloy. The flow stress decreases with the increase of deformation temperature and increases with the increase of strain rate. The hyperbolic sine form of Zener-Hollomon parameter Describe the flow stress behavior of 70 75 aluminum alloy during high temperature compression deformation
其他文献
下午,我在外婆家闲着没事干,便想跟舅舅玩一玩磨“蚂蚱”比赛。我说了自己的想法后,想不到舅舅这个“大小孩”非常乐意。于是,我便去村头的草丛里拔来几株马尾草当“蚂蚱”。
本文对热法磷酸塔内的传热及反应过程进行了数值模拟研究,针对云南省磷化工中试基地所提供的磷酸塔的设计结构,探讨了喷磷量的变化及过量空气系数对磷酸塔壁面平均热流、最大
凌宗伟校长一直认为自己最拿手、最顺手的是上课。但有地方请他作讲座,或者有什么人到学校来学习交流,凌校长总是很干脆地说:“来吧,我给你们上一节课。”凌校长能这样“大言不惭
【人物名片】凌宗伟,1958年生,中学高级教师,语文特级教师,现为江苏省南通市通州区二甲中学党总支书记、校长;南通市学科带头人,通州市专业技术拔尖人才,南通市新世纪科学技术带头人
留意一下,你会发现,很多地方都有这么两条触目惊心的红线,车站、码头、窗口、公园入口……它是要测量什么呢?出口处,人头攒动,刚刚下车的旅客,蜂拥而出。
阳春三月,春光明媚。为庆祝德国劳力士钢琴进军中国市场及霍普菲德生产基地的投产使用。德国劳力士钢琴(中国)有限公司首次在广州举行劳力士经销商大会。会议期间,公司负责人与到
多年前,在萨拉热窝那场悲剧性的战争中,一名记者正在街头用笔记录着这座城市的硝烟和破败。正在这时,他看到了一个被狙(ju)击手射中的小女孩。记者赶紧扔下手中的记事本和铅笔,
夏末秋初是山林探险的好季节,我和几位驴友一起,来到了贵川交界处的一个偏僻深山里探险旅游。走进山林后的第三天,我们无意中发现了一座只有十来间泥砖房的小村子,在村外的空
一位15岁的少女写信问道:“怎样做才能让自己的生活变得充实而有意义?”下文是对这一问题的回答。
介绍了钢包顶渣改质剂在50 t LF炉精炼含铝16MnR钢时的应用,研究结果表明:应用试验钢包顶渣改质剂后,在钢成品中铝含量满足成分要求的基础上,加强了钢液的深脱硫和脱磷,并降