在压力容器产品监督检验过程中,好多人为焊接工艺评定和产品焊接试板的冲击试验试验温度和合格指标争论不休,主要的焦点集中在容器板如16MnR的冲击试验温度和合格指标上。大家知道,GB 6654—1996《压力容器用钢板》第二号修改单对16MnR原材料的冲击试验温度和合格指标作了修改,分别为0℃和31J。于是有人就认为16MnR焊接工艺评定和产品焊接试板的冲击试样也应该做0℃冲击,冲击功不小于31J为合格。其实不 During the supervision and inspection of pressure vessel products, many people have been debated the impact of welding process qualification and impact test of product welding test panels on the test temperature and the qualification index. The main focus is on the impact test temperature and the conformity index of the container panel such as 16MnR. We all know, GB 6654-1996 “Pressure Vessel Steel Plate” Second Amendment to 16MnR raw material impact test temperature and compliance indicators were modified, respectively 0 ℃ and 31J. So some people think 16MnR welding process assessment and product welding test specimens should also do 0 ℃ impact impact, impact power is not less than 31J qualified. Actually not
其他文献
冷却水系统是一个特殊而复杂的生态环境,适合于多种微生物的生长.人们在生产实践安中对微生物的生长及造成的危害现象已有较为充分的认识,如工业循环冷却水的冷却塔池布满绿
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生、测量监控等方面人手,介绍了S226海滨大桥
叙述了实施钢瓶焚烧的原因,提出了钢瓶焚烧炉的基本结构及焚烧工艺。通过理论和实践并经过数据分析证明钢瓶焚烧工艺是可行的,且钢瓶焚烧工艺的过程和结果符合标准规定。
利用拉伸试验方法研究了应变强化对焊接缺陷裂纹的影响,试验分析了不同的应变量、不同方向的应变强化对裂纹缺陷的影响,结果表明:3%应变强化使裂纹缺陷增长了30%,6%应变强化
合成氨工业是我国的一种传统工业,随着社会经济和科学技术的不断发展,合成氨工业面临着大规模的升级转型.要想做好传统合成氨工业的转型升级,就必须综合各方面因素,从原料路
该文从挂篮荷载计算、施工流程、支座及临时固结施工、挂篮安装及试验、合拢段施工、模板制作安装、钢筋安装、混凝土的浇筑及养生、测量监控等方面人手,介绍了S226海滨大桥
提高疗效和降低副反应是药物研发的两大问题.β-榄香烯的药理活性研究是对β-榄香烯进一步开发利用的必然途径.本文对β-榄香烯的药理活性进行了介绍,并对其进一步开发和利用
上个世纪90年代初,我们开始对上海锅炉制造厂的部分锅炉产品进行监督检验.随后监督检验范围逐步扩大,锅炉的压力等级也逐步提高.至2002年底,锅炉产品监督检验的范围已扩大到4
为比较管板在不同形式管孔下的应力强度,分别在UG中建立了八分之一模型,即圆形开孔和椭圆形开孔的管板结构。在ANSYS中进行温度场和应力场的的分析。对计算结果进行分析,结果
本文对影响贫油含苯各个因素进行了分析,并论述了采取相应措施后贫油控制方面的积极影响.其中对提高蒸汽流量后贫油含苯变化趋势进行统计,效果明显,值得推广;同时对贫油含苯