论文部分内容阅读
针对球铁铸管内壁渣多、延伸率合格率低、压扁率合格率低等问题,应用低稀土低硅球化剂进行了实验,结果显示:球铁铸管渣量减少,延伸率合格率、压扁率合格率分别提高了25.3% 和19.4% 。
In view of the problems that the inner wall of the ductile iron pipe has a lot of slag, the pass rate of the elongation is low and the pass rate of the calendaring is low, the experiment was carried out by using the low-rare earth low-silica nodulizer. The results showed that: Rate, crush rate of pass rate increased by 25.3% and 19.4%.