Density Measurement of Liquid Ni-Ta Alloys by a Modified Sessile Drop Method

来源 :Journal of Wuhan University of Technology-Materials Science | 被引量 : 0次 | 上传用户:lihonggeng
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
The density of liquid Ni-Ta alloys was measured by using a modified sessile drop method. It is found that the density of the liquid Ni-Ta alloys decreases with the increasing temperature, but increases with the increase of tantalum concentration in the alloys. The molar volume of liquid Ni-Ta binary alloys increases with the increase of temperature and tantalum concentration. The density of liquid Ni-Ta alloys was measured by using a modified sessile drop method. It is found that the density of the liquid Ni-Ta alloys decreases with the increasing temperature, but increases with the increase of tantalum concentration in the alloys. molar volume of liquid Ni-Ta binary alloys increases with the increase of temperature and tantalum concentration.
其他文献
据《南方日报》报道,今年6月29日下午16时45分,深圳东部华侨城大峡谷探险乐园的太空迷航项目设备突然发生重大安全事故,6人抢救无效身亡,10人受伤。目前该起事故还在调查中,
A wear resistant (Cr,Fe)7C3/γ-Fe ceramal composite coating was fabricated on substrate of a 0.45% C carbon steel by plasma transferred arc (PTA) cladding proce
A novel measurement method for chemical solubility determination is brought forward, in which the advantages of two kinds of traditional methods are united. The
特优奖南通市通州区联络站江阴市联络站常州市武进区联络站兴化市联络站泰兴市联络站常熟市联络站常州市联络站海门市联络站上海浦东新区新四军历史研究会联络站宜兴市联络站
10月26日,由中国民用航空运输协会飞行乘务委员会主办,厦门航空有限公司协办的中国航协飞行乘务员委员会二届三次会议暨“提高客舱安全服务管理”研讨会在厦门举行。民航局副
随着我国建筑业的发展,在建筑施工中减少事故发生,保护国家财产和人民生命安全已成为建筑行业的一件大事。因此,开展对建筑施工项目的安全风险控制与安全管理模式的研究有着
辊压机液压站由于油泵磨损,出口压力降低,满足不了辊压机的工作要求。据此本着国产替代进口的原则,进行了如下改造。 原齿轮泵的工作压力为 15.5MPa,流量241/min,电机功率为7.5kw。 现加一台轴向柱塞
7月23日晚8时30分左右,北京开往福州的D301次动车,行驶到浙江温州永嘉至温州南区间时,与杭州开往福州南的D3115次动车追尾相撞。据报道D31 15次动车疑因遭雷击后失去动力停车
This research has investigated the in-situ Ti alloying of aluminum alloys and its application to A356 alloys and wheels through the evaluation of microstructure