Micro Patterning, Tension Force and the Growth of Osteoblasts

来源 :2014中国功能材料科技与产业高层论坛 | 被引量 : 0次 | 上传用户:jane_89
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
  The microenvironment has been shown to regulate cellular functions including cell growth, differentiation, proliferation, migration, cancer development and metastasis.
其他文献
An iron based composite coating reinforced by (Fe,Cr)7C3 particles, with a thickness of 4.0 mm,was fabricated on the ductile castiron substrateby means of a centrifugal casting and in situ techniques.
Thermal insulation exterior wall coating has been successfully prepared, using styrene-acrylic emulsion as film former, and xonotlite as heat-insulating filler,which produced by hydrothermal reaction.
金属镁具有高反应活性,燃烧释放热值高,因此被广泛应用于火炸药领域。本文主要研究镁粉粒径及含量对聚四氟乙烯热分解的影响规律,选用两种不同粒度的镁粉进行对比,利用TG-DSC同步热分析仪研究不同升温速率下镁/聚四氟乙烯含能体系的热行为。
Mg-doped GaN nanowires have been successfully synthesized on Si (111) substrates by magnetron sputtering deposition through ammoniating Ga2O3/Au thin films at 900 ℃ for 15 min.
In this study, hollow glass microspheres (HGM) and hollow polystyrene microspheres (HPSM) have been employed as fillers in epoxy resin to prepare the syntactic foam.A kind of good performance composit
In order to prevent Zn2SiO4:Mn2+with short decay time for 3D plasma display panels (PDPs) from the deterioration of the luminescence efficiency caused by vacuum ultraviolet (VUV) irradiation, MgF2 coa
Self-assembled method for controllable fabrication of a hydrophobic triazine dithiol-silane composite film on 304 stainless steel (SS) is reported in this paper.Hierarchical structure composed of micr
One lanthanide nitrate (Ln =Tb)with a novel three dimensional structure have been prepared through hydrothermal method.Singlecrystal X-ray diffraction structures were obtained.
A monetite coating was deposited on Carbon/Carbon composites(C/C) by a chemical liquid vaporization deposition (CLVD) method, and then hydrothermally conversed to a hydroxyapatite (HA) coating.
本文探讨了无水压裂用烷基磷酸酯凝胶剂的合成条件,确定了最佳酯化温度为85~90℃.反应时间为5h,并用多元醇与聚磷酸酯中间体反应合了成常温下为液态的烷基磷酸酯凝胶剂JED-3S.