Effect of temperature and loading mode on environmentally assisted cracking of a domestic forged 316

来源 :第三届核电厂材料与安全可靠性国际研讨会 (3rd MRNPP Symposium) | 被引量 : 0次 | 上传用户:redlong888
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
  The crack growth rates(CGRs)of a domestic forged nuclear grade 316L SS piping material were measured at various temperatures and loading modes in simulated pressurized water reactor primary water environment using compact tension specimens.In this work,the simulated recirculating PWR primary water environment contained 1500 ppm B as H3BO3 and 2.3 ppm Li as LiOH.The ppm or ppb refers to weight percentages in this paper.A direct current potential drop(DCPD)technique was used to monitor CGRs throughout the tests.The fracture surface exhibited typical intergranular stress corrosion cracking(IGSCC)characteristics.CGRs increased monotonically with increasing temperature.CGRs under trapezoidal waveform loading were moderately higher than those under constant K loading.
其他文献
Grain boundary engineering(GBE)was applied to enhancing the stress corrosion cracking(SCC)resistance of 304 stainless steel.After the GBE treatment,the grain boundary network(GBN)was featured by the h
会议
The raw materials is the pivotal role for the U-bending heat-transfer pipe of nuclear power steam generator.800-alloy is nickel base alloy with high strength and high corrosion resistance.It greatly i
Nickel-based alloys such as Alloy 600 and Alloy 690,and weld metals such as Alloys 182/2082/132/52/152 have been widely used in pressurized water reactor(PWR)components.Stress corrosion cracking(SCC)o
会议
Nuclear-grade stainless steels and nickel-base alloys have been extensively used as construction materials in nuclear power industry due to their combined good mechanical properties and corrosion resi
会议
This paper studies the effects of Zn additions on the deposition behavior of Co in oxide films in the simulated PWR primary water environment at 315℃.304 stainless steel was soaked in high temperature
The commercial Alloy 690TT was first immersed in the normal hydrogenated primary water at 325 ℃ and 15.6 MPa for 720h and then immersed in the oxygenated primary water at 325℃ and 15.6 MPa for 720h wi
会议
Steam generation tubing materials have the susceptibility of stress corrosion cracking(SCC)under the severe steam conditions.Alloy 600,Alloy 800 and Alloy 690 are widely used as the steam generation t
会议
The stress corrosion cracking(SCC)behavior f A508/52M part in dissimilar metal weld A508/52M/316L in simulated primary water environments at 290℃ was investigated by means of slow strain rate testing(
The effect of strain rate on stress corrosion cracking of 316LN SS in borated and lithiated(B/Li)high temperature water was studied.The results showed that SCC occurred only in a certain strain rate r
会议
In this paper we studied the effects of temperature and dissolved oxygen on crack growth rate in 316L type stainless steel used as auxiliary pipe in nuclear power systems in high purity water under th