Influence of Preparation Process on Briquette and Form Coke compressive Strength

来源 :The 6th International Conference on Hydrometallurgy(第六届国际湿法冶 | 被引量 : 0次 | 上传用户:WYH5198
下载到本地 , 更方便阅读
声明 : 本文档内容版权归属内容提供方 , 如果您对本文有版权争议 , 可与客服联系进行内容授权或下架
论文部分内容阅读
This paper investigated preparation process of briquette by using starch and bentonite as composite binder.It also studied the impact of pulverized coal particle size, coking particle size, compacting pressures, moisture content on the strength of briquette and form coke.The result showed that coking coal particle size was the main influence factor.And the optimum conditions of molding process were as follows: low rank pulverized coal particle size was less than 0.63mm, coking coal particle size was less than 0.28mm, compacting pressure was 60 kN, molding moisture content was 12%.Under the optimal conditions, compressive strength of briquette and form coke was 3470 N/ball and 2910 N/ball,respectively.
其他文献
Diagnostic leaching is a technique used in gold ore processing to determine the gold deportment of an ore, i.e.the distribution of gold between the different mineral phases composing the ore (Lorenzen
会议
Since 1952, many researches were focused on the recovery of uranium from wet phosphoric acid (WPA) since this unconventional resource was economically attractive as a large part of the capital expendi
会议
The development of projects for the recovery of uranium from unconventional resources has gained considerable importance.Phosphate rocks represent a suitable alternative source for uranium production
会议
Niobium and tantalum are strategic metals for electronic and alloys industries but the development of efficient, economic and environmentally friendly processes to recover them from ores is a challeng
会议
Wet Phosphoric Acid (WPA), whose concentration is typically ranging between 4 and 7 mol.L-1, is a strategic source of uranium that can be exploited in spite of its low uranium content (0.1-0.4 g.L-1)
会议
As one of the most promising gold-leaching alternatives to cyanide, thiourea has been widely studied and applied for gold leaching from different aurous minerals due to its fast leaching kinetics and
会议
Currently, three methods were employed for disposal of arsenic in effluent streams including: (i) Neutralization with the lime; (ii) Co-precipitation with ferric; and (iii) the synthesis of scorodite.
Acid mine drainage (AMD) contains high concentration of metal ions, and it will be easily formed in the presence of Acidithiobacillus ferrooxidans(Li et al., 2009).Quorum sensing is a cell-to-cell com
The high temperature chloridizing roasting is one of useful methods to separate nonferrous metals from pyrite cinder and metallurgy slag.However, as one kind of main nonferrous metals in pyrite cinder
会议
The increasing atmospheric CO2 concentration has led to concerns about global warming[1].Therefore,it is imperative for the societies to face with the serious demand for minimization of CO2 emission.S
会议